1
00:00:00,000 --> 00:00:01,280
Picture a sunny afternoon.

2
00:00:01,400 --> 00:00:06,240
You've softwashed a rendered gable, it
looks fantastic, and you're packing up.

3
00:00:06,384 --> 00:00:09,920
Then the customer points at the bifold
door frame and says,

4
00:00:10,000 --> 00:00:11,360
"What's that milky streak?"

5
00:00:11,540 --> 00:00:12,880
You wipe it.

6
00:00:12,987 --> 00:00:14,000
It doesn't wipe.

7
00:00:14,128 --> 00:00:17,440
That's etched aluminium, and it's not
coming back.

8
00:00:17,458 --> 00:00:21,778
Hello, I'm Mark Cave from SoftWash UK, and
today we're talking about cleaning around

9
00:00:21,858 --> 00:00:24,098
metals without causing reactions.

10
00:00:24,218 --> 00:00:29,698
Aluminium, lead, copper, zinc, stainless
steel, and painted or powder coated

11
00:00:29,751 --> 00:00:30,778
metalwork.

12
00:00:30,866 --> 00:00:32,978
Most of us survey the wall or the roof.

13
00:00:33,138 --> 00:00:35,938
Far fewer of us survey the metal sitting
on it.

14
00:00:35,958 --> 00:00:38,118
Let's start with why metals are
vulnerable.

15
00:00:38,198 --> 00:00:42,198
Sodium hypochlorite, SH, is a powerful
oxidiser.

16
00:00:42,246 --> 00:00:44,518
That's exactly why it kills algae so well.

17
00:00:44,678 --> 00:00:49,478
But oxidising is a chemical reaction, and
when SH lands on metal,

18
00:00:49,498 --> 00:00:51,158
the metal reacts too.

19
00:00:51,238 --> 00:00:56,118
You can get pitting, discolouration and
staining, and it can start straight away.

20
00:00:56,125 --> 00:00:59,005
Each metal reacts in its own way, so let's
go through them.

21
00:00:59,165 --> 00:01:04,205
Lead flashing turns dark brown, what we
call scorched, because of lead dioxide

22
00:01:04,255 --> 00:01:05,485
forming on the surface.

23
00:01:05,725 --> 00:01:10,205
If you listened to our earlier episode on
pink UPVC and scorched lead,

24
00:01:10,225 --> 00:01:11,325
you'll know that reaction.

25
00:01:11,432 --> 00:01:13,885
Today is about stopping it before it
starts.

26
00:01:13,917 --> 00:01:17,517
Bare aluminium, so window trims, copings
and bifold frames,

27
00:01:17,597 --> 00:01:18,717
oxidises quickly.

28
00:01:18,877 --> 00:01:22,477
It etches, and you get those milky white
streaks or a pitted,

29
00:01:22,517 --> 00:01:23,197
hazy look.

30
00:01:23,309 --> 00:01:25,757
That's the one you can't simply wipe away.

31
00:01:25,792 --> 00:01:30,912
Zinc and galvanised steel, so gutters,
downpipes and architectural cladding,

32
00:01:30,965 --> 00:01:33,792
react strongly to chlorine and to acidic
cleaners.

33
00:01:33,932 --> 00:01:38,992
You can strip the protective layer and end
up with mottled black or white oxidation.

34
00:01:39,141 --> 00:01:44,512
Copper and brass, think downspouts, bell
pushes and exterior lighting,

35
00:01:44,560 --> 00:01:48,752
tarnish quickly to a greenish black patina
when they meet strong oxidisers.

36
00:01:48,792 --> 00:01:51,192
And then painted and powder coated metal.

37
00:01:51,405 --> 00:01:57,512
If that coating is aged, thin, or already
weakened by UV, hypochlorite or even a

38
00:01:57,576 --> 00:02:01,032
surfactant can cause dulling, chalking, or
edge lifting.

39
00:02:01,312 --> 00:02:03,712
A good coating usually copes.

40
00:02:03,812 --> 00:02:05,912
A tired one often doesn't.

41
00:02:06,012 --> 00:02:09,352
And from the ground, you can't always tell
which you've got.

42
00:02:09,375 --> 00:02:13,455
So, before you touch the chemical rig, do
a metal survey.

43
00:02:13,503 --> 00:02:17,535
Walk the whole elevation and list every
piece of architectural metal.

44
00:02:17,581 --> 00:02:18,455
Window sills.

45
00:02:18,515 --> 00:02:19,855
Bifold door tracks.

46
00:02:19,895 --> 00:02:20,415
Flashings.

47
00:02:20,508 --> 00:02:22,415
Metal soil pipes and vents.

48
00:02:22,495 --> 00:02:23,535
Outdoor lights.

49
00:02:23,581 --> 00:02:24,735
Copper eaves.

50
00:02:24,775 --> 00:02:26,495
Aluminium composite cladding.

51
00:02:26,522 --> 00:02:28,415
If it's metal, it goes on the list.

52
00:02:28,417 --> 00:02:32,097
Then, and this one gets overlooked, follow
the runoff path.

53
00:02:32,257 --> 00:02:36,337
Ask yourself where the chemical goes after
it leaves the wall or roof.

54
00:02:36,577 --> 00:02:41,617
A roof wash can run down onto a lead
valley, a zinc box gutter or a copper bay

55
00:02:41,686 --> 00:02:42,977
canopy below.

56
00:02:43,077 --> 00:02:46,817
You might never have sprayed those
directly, but the runoff gets there anyway.

57
00:02:46,945 --> 00:02:50,817
That's one of the most common ways people
cause damage without realising.

58
00:02:50,833 --> 00:02:52,113
Now the protection protocol.

59
00:02:52,233 --> 00:02:56,073
First, wet the metal with clean water
before you apply anything.

60
00:02:56,173 --> 00:02:57,073
Saturate it.

61
00:02:57,185 --> 00:02:59,793
That water acts as a sacrificial barrier.

62
00:02:59,913 --> 00:03:04,273
Any drift or overspray that lands on a wet
surface is diluted straight away,

63
00:03:04,313 --> 00:03:06,753
instead of sitting on bare metal at full
strength.

64
00:03:06,792 --> 00:03:10,152
Second, mask the high value or unprotected
pieces.

65
00:03:10,332 --> 00:03:15,432
Raw aluminium trims, delicate zinc
capping, an untreated copper lantern.

66
00:03:15,560 --> 00:03:17,512
Tape them and cover them with sheeting.

67
00:03:17,672 --> 00:03:21,992
It takes a few minutes, and it's far
cheaper than a replacement part and an awkward

68
00:03:22,032 --> 00:03:22,552
phone call.

69
00:03:22,583 --> 00:03:24,503
Third, keep a rinse line active.

70
00:03:24,631 --> 00:03:28,423
When you're spraying walls or roofs next
to metal, have somebody on the ground

71
00:03:28,485 --> 00:03:30,983
continuously wetting and flushing the
metalwork.

72
00:03:31,143 --> 00:03:34,744
If you're on your own, plan your sequence
so you can rinse as you go.

73
00:03:34,844 --> 00:03:38,904
The aim is simple: the chemical never gets
time to dwell on the metal.

74
00:03:38,917 --> 00:03:41,557
And fourth, rinse straight after
application.

75
00:03:41,664 --> 00:03:44,277
Never let softwash chemical dry on metal.

76
00:03:44,517 --> 00:03:48,437
Drying concentrates it, and on a powder
coated frame in direct sunlight,

77
00:03:48,469 --> 00:03:51,717
that quick evaporation can leave permanent
chemical burn marks.

78
00:03:51,957 --> 00:03:55,717
So think about the sun on the elevation,
not just the wind.

79
00:03:55,750 --> 00:03:58,230
Let's cover a few mistakes I see
contractors make.

80
00:03:58,350 --> 00:04:03,110
One is treating rust or efflorescence with
acids, such as oxalic or brick acid,

81
00:04:03,177 --> 00:04:05,350
close to galvanised steel or bare
aluminium.

82
00:04:05,563 --> 00:04:07,670
Acids and those metals don't get on.

83
00:04:07,870 --> 00:04:11,110
The other is mixing acids anywhere near
SH.

84
00:04:11,174 --> 00:04:14,310
That's a toxic chlorine gas hazard, and
it's a serious one.

85
00:04:14,422 --> 00:04:18,470
Keep them separate, in storage, in mixing
and on the wall.

86
00:04:18,500 --> 00:04:19,620
Then there's a business point.

87
00:04:19,700 --> 00:04:23,220
Before you quote or spray, photograph
what's already there.

88
00:04:23,318 --> 00:04:25,620
Existing oxidation on aluminium.

89
00:04:25,753 --> 00:04:27,220
Chalking on a powder coat.

90
00:04:27,380 --> 00:04:29,940
Old runoff corrosion under a lead
flashing.

91
00:04:30,153 --> 00:04:35,220
If a customer later says you caused it,
dated photos from before you started are the

92
00:04:35,284 --> 00:04:36,740
best protection you've got.

93
00:04:36,960 --> 00:04:40,900
And if the metal is already in poor
condition, tell the customer,

94
00:04:40,953 --> 00:04:43,060
in writing, before the work starts.

95
00:04:43,083 --> 00:04:44,123
Here's the bigger message.

96
00:04:44,299 --> 00:04:47,483
Most of these problems aren't product
failures.

97
00:04:47,579 --> 00:04:52,123
They come from not knowing what you're
looking at, or not having a workflow.

98
00:04:52,219 --> 00:04:54,683
Knowledge comes before chemicals.

99
00:04:54,763 --> 00:05:00,123
Understand the surface, understand the
reaction, and the damage mostly prevents

100
00:05:00,203 --> 00:05:00,763
itself.

101
00:05:00,792 --> 00:05:02,552
Podcasts like this are a good start.

102
00:05:02,632 --> 00:05:05,912
But if you're serious about offering
softwashing professionally,

103
00:05:05,952 --> 00:05:11,672
the CPD Certified Softwash Training Course
at softwashing.uk goes much deeper into

104
00:05:11,732 --> 00:05:17,112
surface identification, chemical
selection, application, safety and pricing.

105
00:05:17,379 --> 00:05:19,912
It's online, so you learn at your own
pace.

106
00:05:20,045 --> 00:05:24,872
It was built from real industry experience
to help contractors avoid expensive

107
00:05:24,934 --> 00:05:25,512
mistakes.

108
00:05:25,672 --> 00:05:30,632
And completing it gives you the chance to
become an Approved Softwash Applicator,

109
00:05:30,648 --> 00:05:34,712
with a directory listing, and to join the
National Association of Softwash

110
00:05:34,768 --> 00:05:35,432
community.

111
00:05:35,458 --> 00:05:37,378
So here's your challenge for the next job.

112
00:05:37,492 --> 00:05:43,378
Before you mix a drop of chemical, walk
the elevation and count the metals.

113
00:05:43,445 --> 00:05:44,498
Write the list down.

114
00:05:44,585 --> 00:05:45,778
Photograph them.

115
00:05:45,906 --> 00:05:50,018
Then plan how each one gets wetted,
covered and rinsed.

116
00:05:50,258 --> 00:05:54,658
Do that every time and you'll avoid most
of the reactions we've talked about today.

117
00:05:54,667 --> 00:05:56,987
Thanks for listening, and I'll catch you
in the next one.